Composite Patch Repair of a Cracked Pipe in ANSYS: Fatigue Crack Growth under Cyclic Pressure

€189,00 €199,00
Optional extras

Need a full custom project? See the options below.

€189,00 €199,00
Optional extras

Need a full custom project? See the options below.

8 people watching this product now!

Material Includes

  • PDF tutorial (12 pages)
  • ANSYS APDL input files: six ready-to-run growth decks (unrepaired and [90]2 to [90]16 patches)
  • Python scripts: deck generator, comparison with the paper, image generator
  • Crack growth results for all six cases with comparison charts
  • Raw ANSYS mesh and contour images at five growth steps
  • README with run instructions

Audience

  • Pipeline and integrity engineers evaluating composite repairs of cracked pipes
  • FEA engineers who need a 3-D fatigue crack growth workflow in ANSYS APDL
  • Researchers and MSc/PhD students in fracture mechanics and composite repair
  • Engineers learning VCCT and Paris-law crack growth

What You Will Learn?

  • Build a 3-D ANSYS APDL model of a cracked pipe repaired with a glass/epoxy composite patch.
  • Compute stress intensity factors along a through-wall crack front with MVCCT.
  • Grow the crack automatically with the Paris law inside one APDL deck, with the mesh following the front.
  • Compare initial K, crack growth, crack-front shape and fatigue life extension with a published ASME paper.
  • Run your own pipe, crack and patch lay-up by changing one Python file.

About Course

A bonded composite patch is one of the fastest ways to keep a cracked steel pipe in service. But how much life does it actually add, and how does the patch change the crack? This ANSYS package answers both questions with a verified 3-D fatigue crack growth model of a pipe repaired with a glass/epoxy patch under cyclic internal pressure. It rebuilds a peer-reviewed ASME study step by step and compares every key result with the paper. You get six ready-to-run APDL decks, Python scripts, all growth results, raw ANSYS images and a 12-page PDF tutorial.

The paper behind the model

Paper title: Fatigue Crack Propagation Analysis of Repaired Pipes With Composite Patch Under Cyclic Pressure
Authors: Mir Ali Ghaffari and Hossein Hosseini-Toudeshky
Journal: ASME Journal of Pressure Vessel Technology, Vol. 135, No. 3, 031402 (2013)
DOI: 10.1115/1.4023568

What the paper studies (our summary): offshore and marine pipes made of low-strength steel such as A537 face both corrosion and cyclic loads, which start corrosion fatigue cracks. The authors repair such a cracked pipe with a glass/epoxy composite patch and run 3-D finite element analyses of crack growth under cyclic internal pressure. An ANSYS APDL program computes the stress intensity factors, grows the crack and updates the mesh automatically. A parametric study shows how patch thickness changes the fatigue life extension and the shape of the crack front. The full abstract is available from the publisher through the DOI link above.

Model at a glance

ItemPaperThis package
PipeA537 steel, Di 198.38 mm, t 10.31 mm, L 2000 mmSame, quarter model with two symmetry planes
CrackAxial through-wall crack, 2a0 = 50 mmSame, grown to 2a = 196 mm
Repair[90]n glass/epoxy patch, FM-73 adhesiveOrthotropic patch, n = 2, 4, 8, 12, 16, plus the unrepaired pipe
LoadCyclic internal pressure ΔP = 20 barSame
Fracture methodVCCT, Paris law, automatic remeshing in APDLMVCCT at 9 front nodes, Paris law da/dN = 6×10−12ΔK2.8578, moving-node mesh in one APDL deck
ElementsSOLID45 / SOLID46SOLID185 (same 8-node formulation), 8 elements through the wall
Mesh through the pipe wall at the crack: pipe, adhesive and composite patch elements, and the whole repaired pipe
The ANSYS model. (a) Elements through the wall at the crack: steel pipe, thin FM-73 adhesive layer and glass/epoxy patch, with the mesh refined on the cracked side. (b) The whole pipe from outside, with the patch wrapped over the crack.

Results compared with the paper

PatchLife extension, restart (ANSYS / paper)Life extension, 63 mm growth (ANSYS / paper)
[90]263.5% / 65.3%137% / 145%
[90]470.8% / 69.6%187% / 181%
[90]878.7% / 76.5%248% / 223%
[90]1286.1% / 83.2%290% / 256%
[90]1693.6% / 90.2%327% / 280%

Comparison graphs: ANSYS vs paper

Crack growth curves of the cracked pipe, ANSYS vs paper
Crack growth curves. Inside crack-tip position against load cycles for the unrepaired pipe and five patch thicknesses. Solid lines: ANSYS. Dashed lines: the paper. Thicker patches slow the crack and stretch the life.
Initial stress intensity factor along the crack front, ANSYS vs paper
Stress intensity factor along the crack front. KI through the wall for the initial 50 mm crack. The patch lowers K most on the patched (outer) side, which is why the front tilts as it grows.
Fatigue life extension versus composite patch thickness, ANSYS vs paper
Fatigue life extension. Life gained by the repair against the number of plies, ANSYS and the paper side by side.
  • Initial stress intensity factor: within −5% to +3% of the paper along the whole crack front for all six cases.
  • Crack-front shape: when the inside tip reaches 90 mm, the patched-side position is within 1.3 mm of the paper.
  • Mesh check: halving the element size at the front changes K by less than 0.4%.
  • Thick patches: for [90]12 and [90]16 our 63 mm life extensions are higher than the paper’s because our fronts settle into an equal-K shape; the tutorial explains this difference.

Crack front and stress images

Images for the unrepaired pipe and the [90]4 and [90]16 patches at 0 to 90 growth steps. Many more views at five growth steps are included in the download.

Crack-front mesh (paper Fig. 5 style)

The mesh moves with the crack front at every growth step. These views show the model and how the front tilts through the wall under the patch.

ANSYS mesh of the composite patch repaired pipe
Whole model: steel pipe, adhesive and patch.
Mesh of the crack region under the composite patch
Crack region on the symmetry plane.
Crack front mesh through the pipe wall, oblique view
Crack front through the wall, oblique view, [90]4, step 50.
Close-up of the crack front mesh after 5 growth steps
Close-up of the front mesh, [90]4, step 5.
Crack front mesh, [90]4 patch, step 50
Crack plane face-on, [90]4, step 50: the patched side lags.
Crack front mesh, [90]16 patch, step 90
Crack plane face-on, [90]16, step 90: a strongly curved front.

Stress contours (raw ANSYS output)

All contours below are ANSYS plots as the solver draws them, with the mesh overlaid on the crack plane.

Hoop stress on the crack plane of the unrepaired pipe
Unrepaired pipe: hoop stress on the crack plane, straight front.
Hoop stress on the crack plane with the [90]16 patch
[90]16 patch: hoop stress on the crack plane, curved front.
Hoop stress at the curved crack front, close-up
Close-up of the stress peak along the curved front, [90]4.
Crack opening and hoop stress on the outside of the unrepaired pipe
Unrepaired pipe: crack opening on the outside surface (magnified).
Fibre direction stress in the glass/epoxy patch
Patch fibre stress: the patch bridges the crack.
Shear stress in the FM-73 adhesive layer
Adhesive shear that transfers load into the patch.
Deformed patched pipe with von Mises stress
Deformed patched pipe, von Mises stress, end of growth.

What is in the download

  • PDF tutorial (12 pages): problem, mesh strategy, MVCCT and Paris-law equations, how to run, results and discussion
  • Six ready-to-run APDL growth decks: unrepaired, [90]2, [90]4, [90]8, [90]12, [90]16
  • Python scripts: deck generator, comparison with the paper, digitised paper data, image generator
  • Crack growth results (growth.txt) for all six cases, comparison charts and a summary JSON
  • Raw ANSYS mesh and contour images for three cases at five growth steps
  • README with run instructions

Who it is for

  • Pipeline and integrity engineers evaluating composite repairs of cracked pipes
  • FEA engineers who need a working 3-D fatigue crack growth workflow in ANSYS APDL
  • Researchers and MSc/PhD students in fracture mechanics and composite repair
  • Anyone learning VCCT, the Paris law and automatic crack growth in ANSYS

Software and requirements

ANSYS Mechanical APDL 2024 R2 or newer (the decks use standard commands and also run in older releases). Python 3 for the scripts. Units are mm, N and MPa. One full growth run takes about 30 to 60 minutes on 4 cores. You need your own copy of the paper for the original text and figures.

Why buy

You get a checked, scripted crack growth model instead of weeks of APDL development: one deck per case, every result compared with a published ASME paper, and a clear tutorial. Change the pipe size, crack length, patch lay-up or step size in one Python file and run your own case. See also composite patch repair of a cracked CT specimen in Abaqus, axial surface cracks in pressurized pipes in ANSYS Workbench and API 579 Level 3 assessment of a cracked pipe in ANSYS.

FAQ

Does it reproduce the paper? Yes. Initial K is within −5% to +3%, life extension at restart within 4 percentage points, and the crack-front shapes match within about 1.3 mm.

Is the paper included? No. The package contains our own model, results and tutorial. The paper is available from ASME through the DOI link.

Can I model my own pipe or patch? Yes. Pipe diameter, wall thickness, crack length, number of plies, material data and growth step are parameters at the top of gen_deck.py.

Why linear elements? The paper uses 8-node SOLID45/SOLID46 elements, so the model does too. A quadratic SOLID186 check with CINT gave the same interior K within about 1%.

Is this a design or acceptance result? No. It is a verified benchmark and training package and does not replace an assessment by a qualified engineer.

Quality guarantee: if you are not satisfied with the delivered product, we will refund you.

Need more than the files?

There are two ways we can help. Book a one hour online consultation if you want to talk a problem through with a CAE engineer, using the checkbox in the order box. Order a project if you need a full simulation built for you, delivered to an agreed scope, price and deadline under a written contract.

We work on FEA and CFD for engineers, researchers and companies. Order your project, or message us on WhatsApp for a quick reply.

Course Content

Product files

  • ANSYS APDL input files
  • PDF tutorial

Reviews

No Review Yet
No Review Yet
€189,00 €199,00
Optional extras

Need a full custom project? See the options below.

8 people watching this product now!

Material Includes

  • PDF tutorial (12 pages)
  • ANSYS APDL input files: six ready-to-run growth decks (unrepaired and [90]2 to [90]16 patches)
  • Python scripts: deck generator, comparison with the paper, image generator
  • Crack growth results for all six cases with comparison charts
  • Raw ANSYS mesh and contour images at five growth steps
  • README with run instructions

Audience

  • Pipeline and integrity engineers evaluating composite repairs of cracked pipes
  • FEA engineers who need a 3-D fatigue crack growth workflow in ANSYS APDL
  • Researchers and MSc/PhD students in fracture mechanics and composite repair
  • Engineers learning VCCT and Paris-law crack growth