A compact-tension (CT) crack specimen in Ansys Mechanical APDL, set up for stress intensity factor (KI) and J-integral extraction at five crack lengths. The geometry and load follow the LPBF Ti6Al4V specimen of Sun et al., Aerospace 2025, 12, 103 (open access, CC BY): 62.5 x 60 x 10 mm block, 5,190 N maximum load, E = 102 GPa. You get five ready-to-run input decks, the saved database, result images and a 4-page PDF tutorial.
What this is, and is not. It is a verified, mesh-converged static model of a straight stationary crack with no residual stress. It is not a validated replication of the paper: it does not include residual stress, crack growth or fatigue life, and our result is about 17 % above the paper curve at the matching crack length (details below).
| Feature | Ansys implementation |
|---|---|
| Mesh | 9,025 SOLID185 bricks, 11,424 nodes; mapped core and radial rings at the crack tip; 1.5 mm far field; 5 layers over the half-thickness |
| Symmetry | Quarter model, about four times smaller than the full specimen |
| Material | Linear elastic, E = 102,000 MPa (paper Table 4); Poisson ratio 0.34 (assumed) |
| Load | 5,190 N as a distributed bearing load on the upper pin semicircle; pins and contact are not modelled |
| Outputs | KI along the front and J-integral (CINT, 8 contours), reaction check, stress field |
| Solve time | 10 to 40 seconds per deck on 4 cores |

| Crack tip a (mm) | KI centre (MPa√mm) | KI thickness average |
|---|---|---|
| 8 | 316.2 | 307.3 |
| 12 (baseline) | 392.5 | 382.7 |
| 14 | 434.0 | 423.3 |
| 17 | 502.0 | 489.5 |
| 20 | 581.9 | 567.1 |

Reading Fig. 10(d) of the paper by eye gives about 335 MPa√mm at the centre line at 10 mm crack extension (our reading, about ±10, not author data). This model gives 392.5 at the matching crack length, about 17 % higher. The paper curve also rises more slowly than this model and the E399 formula, so a simple shift of the crack-length origin does not reconcile them. The paper does not publish the notch and pin dimensions, the crack-length origin or the crack-front shape. We therefore claim no validation against the paper. The straight crack and zero KII and KIII follow from the symmetry.
Does it reproduce the paper? No. It is a verified baseline of a straight stationary crack. It is about 17 % above the approximate paper value at the matching crack length, and the cause is open.
Do I need Workbench? No. Run /INPUT,CT_baseline,apdl in an empty working directory.
Is this a design result? No. It is a training and starting-point model and does not replace an assessment by a qualified engineer.
Need more than the files?
There are two ways we can help. Book a one hour online consultation if you want to talk a problem through with a CAE engineer, using the checkbox in the order box. Order a project if you need a full simulation built for you, delivered to an agreed scope, price and deadline under a written contract.
We work on FEA and CFD for engineers, researchers and companies. Order your project, or message us on WhatsApp for a quick reply.
Other packages engineers working on this topic also download.
Creep Damage Notched Bar in ANSYS APDL: Becker 2002 Benchmark with No User Subroutine, Decks and Paper Comparison€49,00
Tank Wind Buckling in ANSYS: EN 1993-1-6 MNA-LBA Model of a Cylindrical Oil Tank€129,00
Creep Damage of a Welded Steam Pipe Branch in ANSYS APDL: HAZ Failure, All-Hex Mesh and Paper Comparison€149,00
Creep Damage Versus Time in ANSYS APDL: Failure Horizon of a Single Element, No User Subroutine€49,00
DNV-RP-C208 Example 8.9 in ANSYS: Low-Cycle Fatigue of a Tubular T-Joint under Out-of-Plane Load€29,00Need a full custom project? See the options below.

€129,00