API 579 Example 4.2 in Abaqus: Corrosion Mapping of a Metal Loss Pressure Vessel

€99,00 €129,00
Optional extras

Need a full custom project? See the options below.

€99,00 €129,00
Optional extras

Need a full custom project? See the options below.

21 people watching this product now!

Material Includes

  • PDF tutorial document
  • Abaqus CAE files
  • Abaqus INP files
  • Solved ODB result files
  • Python scripts and inspection data

Audience

  • FEA engineers who turn thickness maps into Abaqus geometry
  • Integrity and inspection engineers working with API 579 metal loss
  • Consultants who want a traceable, checked example
  • MSc and PhD students working on corroded vessels and pipelines

What You Will Learn?

  • Reproduce the Level 1 and Level 2 arithmetic of API 579 Example 4.2 from the raw inspection grid.
  • Turn a 7 x 8 thickness grid into a 3D Abaqus solid wall with internal metal loss.
  • Keep all 56 readings exact, with a fixed outer surface and no smoothing.
  • Apply pressure and closed-end thrust correctly to a thinned vessel.
  • Build current and five-year wall models and compare their response.
  • Run a mesh study and read the results without trusting a single peak stress.
  • Check the model geometry against the inspection data: readings, volume and element quality.
  • Understand what a pressure-only global proof-load run does and does not prove.
  • Know the limits of the model before using the method on a real assessment.

About Course

An inspection report gives you a grid of thickness readings. API 579 Level 1 and Level 2 turn that grid into a few numbers and a pass or fail. They do not show you the thinned wall, and they do not show how the vessel really responds to pressure.

This package takes API 579 Example 4.2 and goes one step further in Abaqus. It reads the 56 inspection readings, builds a full 3D model of the pressure vessel with the internal metal loss in place, and solves it at 300 psig. It does this twice: once for the wall as measured, and once for the wall five years later. Then it checks, number by number, that the model matches the inspection data.

Abaqus corrosion mapping of API 579 Example 4.2: full vessel displacement, von Mises stress patch and mapped solid wall mesh
Corrosion mapping in Abaqus: from 56 thickness readings to a solved 3D vessel model.

What this package is about

Corrosion mapping means turning a table of remaining-wall readings into real geometry that a finite element solver can use. Done by hand, it is slow and easy to get wrong. Here the whole chain is open and repeatable:

  • Measure — the 7 x 8 inspection grid of API 579 Example 4.2.
  • Reconstruct — a solid Abaqus wall, with the outer surface fixed and the inner surface following the remaining thickness.
  • Solve — current wall and five-year wall, with Abaqus CAE, INP and ODB files for every case.
  • Check — the wall recovered from the solved model is compared with the original readings, and the API Level 1 and Level 2 arithmetic is recalculated.

The package comes with a PDF tutorial that walks through each step.

The API 579 Example 4.2 problem

We describe the example in our own words. The standard itself is not included, so keep your copy of API 579-2 / ASME PTB-14 next to you if you want to read the original. A steel pressure vessel has local metal loss on the inside. The wall was measured on a grid with 1.5 in spacing, and the question is whether the vessel can keep operating for another five years at a known corrosion rate.

Inputs of the example

MaterialSA-516 Grade 70 (1999)
Inside diameter48 in
Nominal wall thickness0.75 in
Height10 ft (120 in)
Design pressure and temperature300 psig at 350 °F
Allowable stress20,000 psi
Weld joint efficiency0.85
Corrosion rate and forecast0.02 in/year for 5 years (0.10 in of future loss)
Inspection grid7 rows x 8 columns, 1.5 in spacing, 56 readings

The 56 inspection readings (remaining wall, inches)

Columns C1 to C8 run along the vessel axis. Rows M1 to M7 run around the circumference. The thinnest reading is 0.36 in at M4 / C5.

 C1C2C3C4C5C6C7C8
M10.750.750.750.750.750.750.750.75
M20.750.480.520.570.560.580.600.75
M30.750.570.590.550.590.600.660.75
M40.750.610.470.580.360.580.640.75
M50.750.620.590.580.570.480.620.75
M60.750.570.590.610.570.560.490.75
M70.750.750.750.750.750.750.750.75

What the example concludes

After five years of corrosion the thinnest point drops from 0.36 in to 0.26 in. The average thickness over the averaging length is 0.426 in, which leaves 0.326 in after the allowance. That is below the wall the Level 1 check requires (about 0.436 in) and below the wall the Level 2 check requires (about 0.392 in). So both averaged-thickness checks fail, while the minimum-thickness check passes.

We recalculated all of it from the raw readings. The results agree with the manual at the precision the manual prints:

ResultAPI manualOur calculation
Averaging length2.564 in2.56411 in
Measured average thickness0.426 in0.42624 in
Available average after allowance0.326 in0.326 in
Level 1 required hoop wall0.436 in0.43562 in
Level 2 required hoop wall0.392 in0.39164 in
Level 1 averaged-wall decisionNot satisfiedNot satisfied
Level 2 averaged-wall decisionNot satisfiedNot satisfied
Minimum thickness checkSatisfiedSatisfied

One detail we kept honest: the manual uses 0.430 in in one place and 0.436 in in another for the minimum-thickness threshold. We recorded both in the package documentation. The outcome is the same either way, because 0.260 in passes both.

Table comparing API 579 Example 4.2 manual values with the recalculated Level 1 and Level 2 results
API 579 Example 4.2: manual values and our recalculation, side by side.

What we built in Abaqus

  • A full-height solid vessel wall. The model is the straight 48 in cylinder with its full circumference, meshed with solid elements. Heads, nozzles and supports are not in the example, so they are not invented.
  • Real internal metal loss. The outer radius stays fixed. The inner surface moves to match the remaining thickness. The removed metal is an unmeshed void, not a deleted element.
  • All 56 readings kept exactly. The wall is interpolated between readings with no smoothing and no overshoot, so no value is invented between the points you measured.
  • Pressure and end thrust. Pressure acts on the real inner faces. The closed-end thrust is applied at the cut end, and the end is free to expand radially.
  • A five-year wall. The 0.10 in allowance (2.54 mm) is removed once from the whole wall. The thinnest point goes from 9.144 mm to 6.604 mm.
  • Several mesh levels. From a coarse mesh of 6,800 elements up to an extra-fine mesh of 355,840 elements, so you can see how results change with refinement.
  • Easy to open. In every damaged model, use the named sets METAL_LOSS_ELEMENTS and CORRODED_INNER_SURFACE to isolate the thinned wall in CAE or in the ODB.
Abaqus solid mesh of a pressure vessel segment with internal metal loss built from inspection readings
Full vessel mesh, remaining wall only, and the internal corroded face.

Results at 300 psig

Same pressure, same vessel. The only change is a thinner wall. These values come from the extra-fine mesh.

QuantityCurrent wallFive-year wall
Minimum wall9.144 mm6.604 mm
Maximum radial displacement of the inspection patch0.148 mm0.166 mm
Radial-column stress metric (convergence diagnostic)138.0 MPa183.1 MPa

The five-year wall moves about 12% more and shows about 33% more stress on this metric. That is the kind of difference a pass or fail number hides.

A warning we put in the package, and repeat here. The highest raw stress sits at a corner of the interpolated map and keeps rising as the mesh is refined. On the current wall it is 138.6 MPa on the fine mesh and 149.7 MPa on the extra-fine mesh. So do not use one peak contour as a decision number. The package shows this mesh effect openly, with a mesh study, so you learn to read it correctly.

The analysis is linear elastic. It uses E = 200,000 MPa, which is a stated modelling assumption and not a measured value at 350 °F. Displacements depend on it. Stresses in this pressure-only elastic analysis do not.

Abaqus von Mises stress at 300 psig for the current wall and the five-year allowance wall
Von Mises stress at 300 psig on the same 0 to 200 MPa scale.
Abaqus displacement of the full pressure vessel at 300 psig, current wall and five-year allowance wall
Full vessel displacement at 300 psig. The two colour scales are separate.
Pressure versus maximum patch radial displacement for the current and five-year Abaqus models at 300 psig
Pressure against patch displacement for both walls.

How the model was checked

A good-looking contour is not proof. These are the checks built into the package, all run on the real INP and ODB files:

  • The API arithmetic. Level 1 and Level 2 results are recalculated from the readings and compared with the manual, as shown above.
  • The geometry. All 56 readings are recovered from the actual mesh coordinates. The largest error is 0.00005 mm. The outer radius stays fixed, every element has a positive Jacobian, and the mesh volume of the inspection patch is within 0.02% of the exact curved map. All ten delivered cases pass.
  • The intact vessel. The undamaged benchmark matches the closed-form thick-cylinder solution within 0.05% on the outer radius.
  • Force balance. The axial reaction balances the applied end thrust to about 0.0001%.
  • Mesh sensitivity. Going from the fine to the extra-fine mesh changes the patch displacement by 0.019% (current) and 0.030% (five-year).
  • The code. The scripts come with 21 passing software tests.
Critical thickness profiles of the API 579 Example 4.2 inspection grid compared with the thickness recovered from the Abaqus mesh
Inspection grid versus the solved Abaqus mesh: the profiles overlap at every reading.
Remaining wall thickness map reconstructed from 56 inspection readings, current and five-year scenario
Remaining wall reconstructed from the 56 readings, current and five-year scenario.

Why map the whole grid

Many simplified methods keep only the thinnest line of readings, called a critical thickness profile. The package shows what that throws away. For the current map, stretching the axial profile across the full circumference removes 81.2% more metal than the real map has lost. Doing the same with the circumferential profile removes 76.0% more.

These alternative geometries were not solved, so this is not a statement about stress or capacity. It simply shows how much of the real damage shape a profile cannot keep.

Full thickness map compared with axial and circumferential critical thickness profile extrusions
The full map compared with two critical thickness profile extrusions.

Pressure-only global proof-load cases

The package also includes two global proof-load runs on the five-year wall, one on the medium mesh and one on the fine mesh. They use a pressure of 405 psig (1.5 x RSFa of 0.9 x 300 psig) and an ideal-plastic analysis strength of 25,500 psi (1.5 x 20,000 x 0.85), applied to the whole component. Both meshes carried the full factored load.

This is a global stability check. It is not a burst pressure, and it does not assess local failure.

What is included

  • PDF tutorial with the full workflow, step by step
  • Abaqus CAE files for the delivered cases
  • Abaqus INP files that match each CAE model
  • Solved ODB result files for ten cases: the intact benchmark, the current wall on four mesh levels, the five-year wall on three mesh levels, and the two global proof-load cases
  • Python scripts and input data (JSON and the 56-reading CSV) used to prepare the model, run the checks and make the plots

Tested with Abaqus 2024. No plugin is needed. Other Abaqus versions are not claimed.

What this package does not do

We would rather tell you now than have you find out later.

  • It is not a full API 579 Level 3 assessment. The manual gives no Abaqus result for this example, so there is no published finite element answer to match. Our stress and displacement results extend the example. The inputs, the Level 1 and Level 2 arithmetic, and the geometry are what we checked against the example.
  • It does not predict burst pressure or remaining life. The five-year wall is a constant allowance, not a corrosion kinetics model.
  • The elastic modulus is an assumption (200,000 MPa), because the example does not supply one at 350 °F.
  • No welds, heads, nozzles or supports. The inspection patch is placed at mid-height as an explicit assumption.
  • Pits between readings are unknown. A 38.1 mm inspection pitch cannot be refined by a finer mesh.

Who this package is for

  • FEA engineers who need to turn thickness maps into Abaqus geometry
  • Integrity and inspection engineers working with API 579 metal loss assessments
  • Consultants who want a traceable, checked example to learn from or cite
  • MSc and PhD students working on corroded vessels and pipelines
  • Anyone who wants to see what a Level 1 and Level 2 fail looks like inside a real model

Software required

You need Abaqus to open the CAE and INP files and to read the ODB results. The package was tested on Abaqus 2024. Ordinary Python 3 is enough for the preparation scripts and the tests.

Frequently asked questions

Is this the actual text of API 579 Example 4.2?

No. It is an independent reproduction. We describe the example in our own words and list its inputs and results. The standard is not included, and it does not replace owning API 579-2 / ASME PTB-14.

Did you match an Abaqus result from the manual?

No, because the manual does not publish one for this example. We matched the manual’s inputs and its Level 1 and Level 2 arithmetic, and we checked that the Abaqus geometry matches the inspection readings. The finite element results are our extension of the example.

Does this replace an API 579 fitness-for-service assessment?

No. A real assessment needs your own asset data, material properties at temperature, load cases and a full review. This package is a training and verification example. Need that assessment on a live vessel? See our FEA and fitness-for-service projects.

Can I use my own inspection data?

Yes, within limits. The package reads a CSV of remaining thickness on a grid (axial offset, circumferential arc, thickness) for the same cylindrical template. The border of the grid must be nominal thickness. Different geometry, material or load cases need your own verification.

Why a solid model and not a shell model?

A solid wall keeps the through-thickness detail and lets you read results at radial layers. It is not automatically more accurate than a well-qualified shell model, and we do not claim that.

Which Abaqus version do I need?

The package was tested on Abaqus 2024 only. Older and newer versions are not claimed.

What if the package is not what I expected?

Write to us. Engineering Downloads refunds clients who are not satisfied with a delivered product.

Related packages and reading

Background reading: understanding API 579 and FFS assessment levels, what assessors expect at API 579 Level 3, corrosion assessment for engineers and pressure vessel stress analysis.

Need more than the files?

There are two ways we can help. Book a one hour online consultation if you want to talk a problem through with a CAE engineer, using the checkbox in the order box. Order a project if you need a full simulation built for you, delivered to an agreed scope, price and deadline under a written contract.

We work on FEA and CFD for engineers, researchers and companies. Order your project, or message us on WhatsApp for a quick reply.

Course Content

Product files

  • Abaqus CAE+INP
  • Tutorial document

Reviews

No Review Yet
No Review Yet
€99,00 €129,00
Optional extras

Need a full custom project? See the options below.

21 people watching this product now!

Material Includes

  • PDF tutorial document
  • Abaqus CAE files
  • Abaqus INP files
  • Solved ODB result files
  • Python scripts and inspection data

Audience

  • FEA engineers who turn thickness maps into Abaqus geometry
  • Integrity and inspection engineers working with API 579 metal loss
  • Consultants who want a traceable, checked example
  • MSc and PhD students working on corroded vessels and pipelines

Related  Products

See more

Want to receive push notifications for all major on-site activities?

✕